Rod:
The production cost of aluminium rod is higher, however, the traditional casting process does not guarantee uniform distribution of aluminium alloy, which easily causes the surface blemish.
Hoonly puts homogeneous aluminium rod to use, and it will reduce die/mold wastage during extrusion, thus improving auminium profile’s surface finish and mechanical property.
Scrub:
Non-scrub treatment is extremely easy to cause surface blemishes.
Hoonly adopts means of frosting oxidized, beauty surface, no blemishes.
Material:
To save costs, some factories use recycling scrap aluminium as the raw material, the produced aluminium profile is usually out of flatness and gray surface even easy to breakage due to the high content of impurities.
Hooly's raw material is A00 standard aluminium ingot that contents 99.99% Al.
Anodized:
To save costs and increase production speeds, some factories reduce anodized time, which causes the thickness of oxidation film not up to standard.
Hoonly products thickness of oxidation film is more than 30% of national standard.
Check:
We have detection tools such as Spectroscope, end face measuring instrument, hardness testing and film thickness measurement etc, there are 12 rigorous testing procedures. Hoonly has been committed to producing high-quality aluminium profiles.
To get more details, please email: hello@hoonly.com
This article was written by Walter Liu on https://www.linkedin.com/pulse/hoonly-aluminium-profiles-features-walter-liu/